I just had a 2001 Sailfish surveyed. A couple of concerns:
There are stress cracks and delamination of the gelcoat, about 2" X 10", with water between the layers on both sides of the transom - upper trailing edges, outside of the motors (twin 200HPDI). Does anyone have a solution to this...